Characteristics:
LKE-NiCrMo-4 is a nickel based low hydrogen type covered electrode which contains less C and Si to reduce carbide precipitation in grain boundary. The excellent heat resistance and corrosion resistance are obtained for chemical plant and FGD equipments
Applications:
It is suitable for HASTELLOY C-276 and dissimilar metal welding.
Notes on Usage:
1.Dry the electrode at 350-400℃ for 30-60 minutes before use.
2.Use small amperage and keep the arc as short as possible
Classification:
AWS A5.11 : | ENiCrMo-4 |
ASME SFA-5.11 : | ENiCrMo-4 |
EN ISO 14172 : | E Ni 6276 |
JIS Z 3224 : | DNiCrMo-4 |
Welding position:
Typical chemical composition of weld metal (wt%)
C | Mn | Si | P | S | Cr | Ni | Nb | Fe | Mo |
0.07 | 0.78 | 0.32 | 0.002 | 0.004 | 20.80 | 59.60 | 3.52 | 5.40 | 8.90 |
Typical mechanical properties of weld metal
YS N/mm2 | TS N/mm2 | EL % | IV -196oC J |
490 | 770 | 38 | 69 |
Sizes and recommended current range (DC+)
Diameter (mm) | 2.6 | 3.2 | 4.0 | |
Length (mm) | 300 | 350 | 350 | |
Amps | F | 65-90 | 70-115 | 95-145 |
V&OH | 60-80 | 60-110 | 80-130 | |
Weight per pack (kg) | 5 | 5 | 5 | |
Weight per carton (kg) | 20 | 20 | 20 |