Stainless Steel Electrodes LKE-NiCrMo-10

▶︎ Characteristics:

Good corrosion-resistance against acetic acid and its anhydride, hot contaminated sulphuric and phosphoric acids and other contaminated oxidizing mineral acids. Intermetallic precipitation is widely prevented.

 


 

▶︎ Applications:

For joining materials of the same and similar nature, e.g. material-no. 2.4602 (NiCr21Mo14W / UNS N06022) and special stainless steels. Furthermore it can be used for dissimilar joints of these alloys with low-alloyed materials and cladding

 


 

▶︎ Notes on Usage:

1. Dry the electrode at 350-400°C for 60 minutes before use.
2. Keep the arc as short as possible.
3. Crater should be ground smooth or crater treatment.

 


 

▶︎ Classification:

AWS A5.11 ENiCrMo-10

 


 

▶︎ Welding position:


 

▶︎ Typical chemical composition of weld metal (wt%)
C Mn Si Cr Mo Ni S W Fe
0.018 0.28 0.19 22.47 14 54.26 0.002 3.21 5.14

 


 

▶︎ Typical mechanical properties of weld metal
TS N/mm² EL % IV -30°C J
770 40 70

 


 

▶︎ Sizes and recommended current range (AC or DC+)
Diameter (mm) 2.6 3.2 4.0 4.8
Length (mm) 300 350 350 350
Amps F 90-120 120-160 160-220 230-300
V&OH 70-110 80-120 110-150 230-300
Weight per pack(kg) 5 5 5 5
Weight per carton (kg) 20 20 20 20